A: The demoulding force is not strong, usually because the viscosity of silicon oil in the die-casting demoulding agent is small. It is suggested to choose the die-casting demoulding agent with strong demoulding force according to the working condition.
A: Generally, the coating problem is caused by the high viscosity of silicon oil in the die-casting release agent. It is suggested to replace the die-casting release agent with a good coating performance.
A: The problem of carbon deposition is generally due to the insufficient temperature resistance of die-casting release agent. Under normal circumstances, the choice of high temperature resistance die-casting release agent can solve the problem.