Atomization quality directly determines the coverage uniformity and evaporation rate of the release agent. Poorer atomization increases the likelihood of die sticking, carbon deposition, and sintering. Under normal conditions, an atomization efficiency below 15% leads to inadequate film formation, whereas an efficiency exceeding 80% ensures satisfactory film formation. This requires comprehensive adjustment in conjunction with spray distance, spray pressure, spray duration, and mold temperature.