Die-casting Release Agent Manufacturer -- KZY new materials CO.,LTD provides you with ultra-high temperature resistance, ultra-thin, anti-oxidation , without silicon or less silicon, universal, powder die-casting release agent, and also provides you with frequently asked questions and technical support.Sitemap
Solutions
Frequent Answers
Popular Articles
Technical Support
Customer Evaluation Cases

How to Solve Sticking the Mold?

Editing time:2022-03-02 ;   Editing by:kzy

Under normal circumstances, sticking to the mold is that because the liquid aluminum pouring speed is too fast, corroding mold cavity. Secondly, because the spraying is not sprayed in place, the liquid aluminum and the mold form adhesion. Of course, if the release agent demoulding performance is poor, there will be sticky mold. We suggesting that in order to ensure the casting quality, you should reduce the pouring speed reasonably, choose the right spraying method, and dilute the release agent according to the proportion required by the artifacts. I hope this is helpful.

For more information about How to Solve Sticking the Mold? or die-casting auxiliary materials, and if you need customized die-casting release agent, please contact 15021483232 (same as Wechat)

Related products
Popular Articles
to Top
15021483232x15021483232@163.com
Copyright(C):Shanghai KZY New Materials Co., LTD.  All Rights reserved.    沪ICP备2022017446号
Shanghai KZY New Materials Co., LTD 
Address:Block A,No.568 Songhong Road,Changning District,Shanghai