When spraying, ensure
even coverage to avoid missed spots or over-spraying. Over-spraying may cause carbon buildup, sintering, or damage the protective film—leading to mold sticking or scratching. Insufficient coverage risks sticking. Additionally, control
spray pressure and distance (adjusted for mold size/shape), and keep the mold surface
clean (free of oil/impurities) to optimize release agent adhesion.